Numerical Simulation and Analytical Prediction of Residual Strength for Elbow Pipes with Erosion Defects

Chao Sun1, Qi Wang1, Yuelin Li1

  • 1School of Measurement and Communication Engineering, Harbin University of Science and Technology, Harbin 150080, China.

Related Concept Videos

Major Losses in Pipes01:28

Major Losses in Pipes

When a fluid flows through a pipe, it experiences energy losses due to frictional resistance along the pipe walls, known as major losses. These energy losses result in a pressure drop, which varies based on the flow conditions — whether laminar or turbulent — and the specific physical properties of the fluid and pipe.
Fluid flow can be classified as laminar or turbulent, primarily based on the Reynolds number. This dimensionless number reflects the relative influence of inertial to...
1.2K
Bending of Material: Problem Solving01:09

Bending of Material: Problem Solving

In this lesson, determine the ratio of the maximum bending moments applied to two metal pipes, given that both pipes can withstand a maximum stress of 100 MPa. Both pipes have an outer radius of 1.8 cm. Pipe A has an inner radius of 1.5 cm, and Pipe B has an inner radius of 1 cm. The ratio of the maximum bending moment applied to two metallic pipes, each with a different inner and outer radius, is determined by considering their dimensions. The inner radius of the first pipe is 1.5 cm, and for...
233
Typical Model Studies01:30

Typical Model Studies

Fluid mechanics model studies often utilize scaled-down systems to predict fluid behavior in full-scale environments, such as river flows, dam spillways, and structures interacting with open surfaces. Maintaining Froude number similarity in river models is crucial, as it replicates surface flow features like wave patterns and velocities.
425
Residual Stresses in Bending01:18

Residual Stresses in Bending

In the study of elastoplastic members subjected to bending moments, understanding the loading and unloading phases is crucial for assessing material behavior and structural integrity. During the loading phase, as the bending moment increases, the material initially responds elastically, adhering to Hooke's Law, where stress is directly proportional to strain. When the load exceeds the yield strength, plastic deformation occurs, resulting in permanent strain and deformation that remains even...
237
Yield Criteria for Ductile Materials under Plane Stress01:25

Yield Criteria for Ductile Materials under Plane Stress

In designing structural elements and machine parts using ductile materials, it is crucial to ensure that these components withstand applied stresses without yielding. Yielding is initially determined through a tensile test, which evaluates the material's response to uniaxial stress. However, tensile stress is insufficient when components face biaxial or plane stress conditions This condition requires advanced criteria to predict failure.
The Maximum Shearing Stress Criterion, also known as...
210
Stresses under Combined Loadings01:23

Stresses under Combined Loadings