Assessment of Poorly Compactable Sands by Recycling and Recompaction: Experimental Program and Packing Particle

Juana Arias-Trujillo1, Agustín Matías-Sánchez1

  • 1Department of Construction, School of Engineering, Universidad de Extremadura, Avda. de la Universidad, s/n, 10003 Caceres, Spain.

Related Concept Videos

Compacting Factor test01:22

Compacting Factor test

The compacting factor test is a method used to assess the workability of concrete. It is  especially suitable for concrete mixes containing aggregates up to one and a half inches in size. This test involves specialized equipment consisting of two truncated cone-shaped hoppers and a cylinder, all with polished interior surfaces to minimize friction.
The procedure begins by placing concrete into the upper hopper without any compaction. Once filled, the bottom door of this hopper is opened,...
222
Design Example: Aggregate Gradation01:24

Design Example: Aggregate Gradation

The right type and quality of aggregates are crucial for concrete as they significantly influence its properties, mix proportions, and cost-effectiveness. If different sources are available for sand, the commonly used fine aggregate in concrete, the selection of sand is primarily based on its gradation.
The grading, or particle-size distribution, of sand is determined using sieve analysis, with standard sizes ranging from 150 μm to 10 mm (ASTM No. 100 sieve to 3⁄8 in. sieve). Sand is...
142
Deleterious Substances in Aggregate01:25

Deleterious Substances in Aggregate

Deleterious substances in aggregates can be detrimental to the quality and durability of concrete. These substances include organic impurities like loam, which interfere with cement hydration and are usually present in the sand. These prevent a good bond between aggregate and cement paste. Organic impurities can be detected using the colorimetric test, where the darkness of a solution after agitation indicates the level of organic content.
Another type of impurity is clay and fine material that...
229
Design Example: Managing Concrete Workability01:14

Design Example: Managing Concrete Workability

This example deals with managing the workability of concrete for a raft foundation project under hot weather conditions. Workability is crucial for ensuring the concrete is easy to place, compact, and finish. In this scenario, a slump test — a common method to measure the workability of fresh concrete — initially indicated low workability. This was attributed to the rapid water loss from the concrete mix, exacerbated by the high temperatures causing the course aggregates to heat up.
109
Unsoundness of Aggregate due to Volume Change01:26

Unsoundness of Aggregate due to Volume Change

Unsoundness in aggregates due to volume changes is primarily caused by the physical alterations aggregates undergo, such as freezing and thawing, thermal changes, and wetting and drying. Unsound aggregates, when subjected to these changes, result in volume change upon disintegration. This, in turn, contributes to the deterioration of concrete, including scaling, pop-outs, and cracking. Particular types of aggregates, such as porous flints, cherts, and those containing clay minerals, are...
156
Slump Test01:20

Slump Test

The slump test is a widely used method to measure the workability of concrete. It employs a 12-inch high truncated cone mold that tapers from eight inches at the base to four inches at the top. Before testing, the mold is securely attached to a flat base and dampened.
Concrete is poured into the mold in three layers to conduct the test. Each layer is compacted 25 times with a steel tamping rod, which has a five-eighths-inch diameter and a rounded end, to ensure even distribution and eliminate...
360