Molybdenum precursor delivery approaches in atomic layer deposition of α-MoO3
Related Experiment Video
Updated: Aug 17, 2025

Solvothermal Synthesis of MIL-96 and UiO-66-NH2 on Atomic Layer Deposited Metal Oxide Coatings on Fiber Mats
Published on: June 13, 2018
Daniela Lorenzo1, David Maria Tobaldi1, Vittorianna Tasco1
1CNR NANOTEC Institute of Nanotechnology, Via Monteroni, Lecce 73100, Italy. david.tobaldi@nanotec.cnr.it.
Abstract:
In this research work, we present a study on time-sequenced plasma-enhanced atomic layer deposition (PE-ALD) processes towards the achievement of high-quality α-MoO3 thin films which are suitable for exfoliation. In particular, a conventional precursor injection method along with a boosted precursor delivery approach are discussed and analysed. In the latter, the proposed gas supply mechanism ensures a large number of deposited Mo atoms per unit of time, which, along with a proper thermal energy, leads to high-quality and oriented orthorhombic α-MoO3 films. The proposed boosted approach is also compared with post growth annealing steps, resulting in more effective achievement of a highly oriented orthorhombic α-MoO3 phase and less time consumption.