Comparative study of temperature effects on white sandstone and rockburst-like materials

Zhengguo Zhu1,2, Chaoyi Ma3, Zhichun Fang3

  • 1State Key Laboratory of Mechanical Behavior and System Safety of Traffic Engineering Structures, Shijiazhuang Tiedao University, Shijiazhuang, Hebei, China.

Plos One
|December 14, 2022
PubMed

Related Concept Videos

Specific Heat01:16

Specific Heat

The specific heat capacity of a substance refers to the energy required to increase the temperature of one gram of that substance by one degree Celcius. Specific heat capacity is often represented in calories (cal), grams (g), and degrees Celsius (oC), but can also be expressed in joules (J), kilograms (kg), and Kelvin (K), among other units.
For example, increasing the temperature of one gram of water by 1°C requires one calorie of heat energy and can be written as 1 cal/g-°C, or...
62.4K
Masonry in Cold and Hot Weather Conditions01:21

Masonry in Cold and Hot Weather Conditions

In cold weather, masonry construction requires specific precautions to ensure mortar does not freeze before curing, as this can significantly weaken its strength and watertightness. Mortar temperature should be maintained between 60°F and 80°F to support proper hydration and curing. Below 40°F, mortar water must be heated, but should not exceed 120°F as high temperatures can reduce mortar's compressive and bond strength.
Other key practices include keeping masonry units...
126
Unsoundness of Aggregate due to Volume Change01:26

Unsoundness of Aggregate due to Volume Change

Unsoundness in aggregates due to volume changes is primarily caused by the physical alterations aggregates undergo, such as freezing and thawing, thermal changes, and wetting and drying. Unsound aggregates, when subjected to these changes, result in volume change upon disintegration. This, in turn, contributes to the deterioration of concrete, including scaling, pop-outs, and cracking. Particular types of aggregates, such as porous flints, cherts, and those containing clay minerals, are...
156
Frost Action on Concrete01:27

Frost Action on Concrete

Concrete structures in cold climates, such as those along roadsides, can retain moisture. This moisture makes them susceptible to frost-related damage when temperatures fall below freezing. Adding moisture worsens the damage during temperature fluctuations, leading to repeated freezing and thawing. De-icing salts, spread over these structures to melt ice, add to the freeze-thaw cycle, and draw even more moisture into the concrete.
This freeze-thaw cycle primarily causes surface scaling, where...
131
Stress-Strain Diagram - Brittle Materials01:24

Stress-Strain Diagram - Brittle Materials

Brittle materials, including glass, cast iron, and stone, exhibit unique characteristics. They fracture without considerable change in their elongation rate, indicating that their breaking and ultimate strength are equivalent. Such materials also show lower strain levels at the point of rupture. The failure in brittle materials predominantly results from normal stresses, as evidenced by the rupture created along a surface perpendicular to the applied load. These materials do not display...
2.7K
Microcracking in Concrete01:20

Microcracking in Concrete

Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
177