All fiber watt-level fiber source at 760 nm generated through four-wave mixing in a photonic crystal fiber
Abstract:
There are limited fiber-based single-mode laser sources over the visible and near infrared range. Nonlinear conversion through four-wave mixing in photonic crystal fibers allows for the generation of new wavelengths far from a pump wavelength. Utilizing an all-fiber spliced configuration, we convert 1064 nm light into a W-level signal in the 750 nm - 820 nm spectral region. We demonstrate over 7.9 watts in the signal band, out of a custom photonic crystal fiber with M2 < 1.15. The input peak power as well as fiber length can be selected to keep the converted power in a 0.6 nm narrow emission band or broaden the output to 45 nm spectral band with spectral density greater than 50 mW/nm by pumping with higher peak powers.
More Related Videos
13:02Fabrication of 1-D Photonic Crystal Cavity on a Nanofiber Using Femtosecond Laser-induced Ablation
Published on: February 25, 2017
08:48Low-cost Custom Fabrication and Mode-locked Operation of an All-normal-dispersion Femtosecond Fiber Laser for Multiphoton Microscopy
Published on: November 22, 2019