Related Experiment Video
Updated: Aug 17, 2025

Solid-state Graft Copolymer Electrolytes for Lithium Battery Applications
Published on: August 12, 2013
A Maximization of the Proton Conductivity of Sulfonated Poly(Ether Ether Ketone) with Grafted Segments Containing
Yang Yu1, Zheng Zeng2, Xuesong Gao1
1Hubei Provincial Key Laboratory of Green Materials for Light Industry, Collaborative Innovation Center of Green Light-Weight Materials and Processing, New Materials and Green Manufacturing Talent Introduction and Innovation Demonstration Base, and School of Materials and Chemical Engineering, Hubei University of Technology, Wuhan, Hubei, 430068, P. R. China.
Abstract:
To enhance the proton conductivity of sulfonated poly(ether ether ketone) (SPEEK), proton-conducting groups are required to be covalently connected to SPEEK and form proton-conducting channels. Herein, SPEEK fully grafted with segments containing multiple, flexible propanesulfonic acid groups (MS-SPEEK-102) is successfully prepared. Compared with SPEEK, MS-SPEEK-102 exhibits a higher proton conductivity of 8.3 × 10-2 S cm-1 at 80 °C with 98% relative humidity, and consequently a greater power density of 0.530 W cm-2 at 60 °C. These can be ascribed to the increased number of sulfonic acid groups, and ample, uninterrupted proton-conducting channels constructed by the movement of the maximum content, flexible side-chain segments. This approach offers an idea for obtaining a proton exchange membrane with good proton conductivity based on SPEEK.
Related Concept Videos
Titration of Polyprotic Acids with a Strong Base
Solvating Effects
Electrophilic Aromatic Substitution: Sulfonation of Benzene
Titration of a Polyprotic Acid
Ion Exchange
Regioselectivity and Stereochemistry of Acid-Catalyzed Hydration