Optical Strain Measurement and Microfractography of the Fractures of Armstal 550 Steel after Temperature Tensile

Paweł Bogusz1, Barbara Nasiłowska2, Grzegorz Sławiński1

  • 1Faculty of Mechanical Engineering, Military University of Technology, Gen. S. Kaliskiego 2, 00-908 Warsaw, Poland.

Related Concept Videos

Mechanical Characteristics of Steel01:18

Mechanical Characteristics of Steel

The mechanical characteristics of steel are assessed through various tests that evaluate its strength, toughness, and flexibility. These tests include tension, torsion, impact, bending, and hardness assessments, each providing crucial information about steel's suitability for specific applications.
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
730
Measurements of Strain01:27

Measurements of Strain

Strain quantifies the deformation of a material under force, typically measured as normal strain, which represents the change in length when compared with the original length. Electrical strain gauges are used for enhanced accuracy. These devices consist of a conductive wire mounted on a paper backing that adheres to the material's surface. These gauges operate on the piezoresistive effect, where the wire's electrical resistance changes in response to mechanical deformation. The strain...
1.9K
Temperature Dependent Deformation01:12

Temperature Dependent Deformation

In a nonhomogeneous rod made up of steel and brass, restrained at both ends and subjected to a temperature change, several steps are involved in calculating the stress and compressive load. Due to the problem's static indeterminacy, one end support is disconnected, allowing the rod to experience the temperature change freely. Next, an unknown force is applied at the free end, triggering deformations in the rod's steel and brass portions. These deformations are then calculated and added...
180
Stress-Strain Diagram - Ductile Materials01:24

Stress-Strain Diagram - Ductile Materials

The stress-strain relationship in ductile materials such as structural steel or aluminium is intricate and progresses through several stages. When a specimen is loaded, it initially exhibits a linear length increase, depicted by a steep straight line on the stress-strain diagram. It indicates the material is elastically deforming and will return to its original shape once unloaded. However, when a critical stress value is reached, plastic deformation begins. This stage sees substantial...
915
Thermal Strain01:19

Thermal Strain

Thermal strain is a concept that arises when we consider how temperature changes affect structures. Unlike the conventional assumption that structures remain constant under load, real-world scenarios often involve temperature fluctuations that can significantly impact these structures. Consider a homogeneous rod with a uniform cross-section resting freely on a flat horizontal surface. If the rod's temperature increases, the rod elongates. This elongation is proportional to the temperature...
2.1K