The carbon footprint of steel corrosion

M Iannuzzi1, G S Frankel2

  • 1Curtin Corrosion Centre, Curtin University, Perth, Western Australia 6845 Australia.

Npj Materials Degradation
|January 3, 2023
PubMed

Related Concept Videos

Corrosion of Reinforcement01:27

Corrosion of Reinforcement

The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
231
Corrosion02:49

Corrosion

The degradation of metals due to natural electrochemical processes is known as corrosion. Rust formation on iron, tarnishing of silver, and the blue-green patina that develops on copper are examples of corrosion. Corrosion involves the oxidation of metals. Sometimes it is protective, such as the oxidation of copper or aluminum, wherein a protective layer of metal oxide or its derivatives forms on the surface, protecting the underlying metal from further oxidation. In other cases, corrosion is...
25.4K
Steel Manufacturing01:26

Steel Manufacturing

Steel manufacturing is a multi-stage process that begins by smelting iron ore into cast iron in a blast furnace. This initial stage involves layering iron ore with coke, a type of fuel, and crushed limestone within the furnace. The coke is ignited with a high volume of air, leading to the creation of carbon monoxide, which acts to reduce the iron ore to pure iron.
During this smelting process, limestone plays a crucial role by forming slag. Slag captures impurities within the molten iron, such...
731
Mechanical Characteristics of Steel01:18

Mechanical Characteristics of Steel

The mechanical characteristics of steel are assessed through various tests that evaluate its strength, toughness, and flexibility. These tests include tension, torsion, impact, bending, and hardness assessments, each providing crucial information about steel's suitability for specific applications.
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
729
Acid Attack on Concrete01:21

Acid Attack on Concrete

When acids come into contact with concrete, they initiate a chemical reaction that dissolves the hydrated cement paste. This process leads to softening and structural weakening of the concrete. This issue is commonly observed in environments such as chimneys, sewers, and industrial settings. The severity of the damage increases as the pH of the water interacting with the concrete drops below 6.5. In particular, a pH under 4.5 can cause significant concrete damage.
The rate at which hydrogen...
300
Carbonation Shrinkage01:24

Carbonation Shrinkage

Atmospheric CO2 penetrates the concrete's pores and, in the presence of moisture, forms carbonic acid, which then reacts with calcium hydroxide in the hydrated cement, forming calcium carbonate. This process reduces the concrete's volume and is termed carbonation shrinkage.