Effect of açai berry extract application on the bond strength to the bleached enamel using an experimental
Lamiaa M Moharam1, Haidy N Salem1, Shahinaz N Hassan1
1Restorative and Dental Materials Department, National Research Centre, Giza, Egypt.
Background:
To evaluate the bleached enamel shear bond strength (SBS) after antioxidants application using an experimental adhesive.
Material And Methods:
Sixty sound human molars had their roots removed then cut into buccal and lingual halves and mounted in acrylic blocks. Enamel bleaching was done using an in-office chemical bleaching agent. Specimens were arbitrarily allocated into 12 groups (n=10) regarding the three experimental levels of the study: two antioxidant agents [10% açai berry extract, 10% sodium ascorbate prepared gels (applied for 15-min) and the control group (no antioxidant application)], two adhesive materials [commercial etch-and-rinse (ER) adhesive and an experimental ER adhesive] and two post-bleaching SBS testing times [24-h and 2-w]. Specimens were restored with a nano-hybrid resin composite restoration then stored in distilled water at 37◦C till SBS testing.
Results:
Three-way ANOVA showed that the antioxidant agents, adhesive materials and the post-bleaching SBS testing times had a statistically significant effect on the bleached enamel SBS. Açai berry extract groups recorded the highest mean values, while the control groups demonstrated the least values with a statistically significant difference between the antioxidant agents' groups. Commercial ER adhesive recorded statistically significant higher SBS values than the experimental adhesive and the 2-w post-bleaching SBS testing time demonstrated statistically significant higher SBS values than the 24-h groups.
Conclusions:
Açai berry extract is a powerful antioxidant agent, that has the potential to instantly restore the bleached enamel depleted SBS. The commercial adhesive has successfully restored the depleted SBS of the bleached enamel than the tested experimental adhesive. Key words:Antioxidant application, açai berry extract, etch-and-rinse adhesives, experimental adhesive, shear bond strength.
More Related Videos
08:20Systematic Approach to Identify Novel Antimicrobial and Antibiofilm Molecules from Plants' Extracts and Fractions to Prevent Dental Caries
Published on: March 31, 2021
08:40Standard Test Method ASTM D 7998-19 for the Cohesive Strength Development of Wood Adhesives
Published on: May 17, 2020
Related Concept Videos
Bonding and Strength of Aggregate
Effects of EDTA on End-Point Detection Methods
In the visual method, metal-ion indicators (metallochromic dyes), which have distinct colors in their free and complex forms, are added to the mixture to signal the titration's end point. They form stable complexes with metal ions, but these complexes are weaker than the corresponding metal–EDTA complexes. As a...