The Activation Energy of Strain Bursts during Nanoindentation Creep on Polyethylene

Mohammad Zare Ghomsheh1, Golta Khatibi1

  • 1Christian Doppler Laboratory for Lifetime and Reliability of Interfaces in Complex Multi-Material Electronics, CTA, TU Wien, Getreidemarkt 9/164, 1060 Vienna, Austria.

Related Concept Videos

Plastic Behavior01:21

Plastic Behavior

A material's elastic behavior is characterized by the disappearance of stress once the load is removed, allowing the material to return to its original state. However, when stress surpasses the yield point, yielding commences, marking the onset of plastic deformation or permanent set. This change from elastic to plastic behavior is influenced by the peak stress value and the duration before the load is removed. An intriguing observation occurs when a specimen is loaded, unloaded, and...
246
Elastic Strain Energy for Shearing Stresses01:20

Elastic Strain Energy for Shearing Stresses

As discussed in previous lessons, strain energy in a material is the energy stored when it is elastically deformed, a concept crucial in materials science and mechanical engineering. This energy results from the internal work done against the cohesive forces within the material. When a material undergoes shearing stress and corresponding shearing strain, the strain energy density, which is the energy stored per unit volume, is calculated. Within the elastic limit, where the stress is...
256
Elastic Strain Energy for Normal Stresses01:22

Elastic Strain Energy for Normal Stresses

Strain energy quantifies the energy stored within a material due to deformation under loading conditions, a fundamental concept in materials science and engineering. The strain energy can be modeled when a material is subjected to axial loading with uniformly distributed stress. In this scenario, the stress experienced by the material is the internal force divided by the cross-sectional area, and the strain induced is directly proportional to this stress through the modulus of elasticity.
If...
237
Strain-Energy Density01:20

Strain-Energy Density

Understanding the strain energy density in materials under axial load is crucial for evaluating their mechanical behavior and durability. When a rod is subjected to such a load, it elongates and stores energy, known as strain energy, as potential energy within the material. This energy is measured in terms of energy per unit volume.
In the elastic region of a material, the relationship between the stress and the strain is linear and follows Hooke's Law. The strain energy density in this...
514
Strain Energy01:13

Strain Energy

Strain energy is a fundamental concept in the field of materials science and structural engineering, describing the energy absorbed by a material or structure when it is deformed under load.
Consider a rod that is fixed at one end and subjected to an axial force at the free end. This axial force induces stress within the rod, leading to its elongation. As the axial force increases, so does the elongation of the rod, illustrating a direct relationship between the force applied and the resulting...
548
Strain and Elastic Modulus01:15

Strain and Elastic Modulus

The quantity that describes the deformation of a body under stress is known as strain. Strain is given as a fractional change in either length, volume, or geometry under tensile, volume (also known as bulk), or shear stress, respectively, and is a dimensionless quantity. The strain experienced by a body under tensile or compressive stress is called tensile or compressive strain, respectively. In contrast, the strain experienced under bulk stress and shear stress is known as volume and shear...