Effect of CO2 on the Desulfurization of Sintering Flue Gas with Hydrated Lime
Jianguo Hong1,2, Xinqing Zou1, Ziqiang Qin1
1State Key Laboratory of Advanced Special Steel & Shanghai Key Laboratory of Advanced Ferrometallurgy & School of Materials Science and Engineering, Shanghai University, Shanghai 200444, China.
Abstract:
The effect of carbon dioxide (CO2) on the desulfurization of sintering flue gas with hydrate (Ca(OH)2) as an absorbent was investigated, and the formation of calcium carbonate (CaCO3) and its effect on the desulfurization was discussed. The competitive relationship between carbon dioxide (CO2) and sulfur dioxide (SO2) with the deacidification agent in sintering flue gas is discussed thermodynamically, showing that sulfates are more likely to be generated under high oxygen potential conditions and that SO2 reacts more preferentially than CO2 under a thermodynamic standard state. The amount of produced CaCO3 increases under the condition that the CO2 concentration is absolutely dominant to SO2 in the sintering flue gas atmosphere. The effect of temperature, humidity and CO2 concentration on the desulfurization of Ca(OH)2 are discussed experimentally. The increasing temperature is not conducive to desulfurization, and the humidity can promote desulfurization, while excessive humidity could inhibit desulfurization. The suitable relative humidity is 20%. In situ generated calcium carbonate has a certain desulfurization effect, but the desulfurization effect is not as good as Ca(OH)2. However, a large proportion of CaCO3 was produced in the desulfurization ash under the condition that CO2 concentration was absolutely dominant to SO2 in the sintering flue gas atmosphere.
More Related Videos
Related Concept Videos
Hydration of Cement
Strength and Heat of Hydration
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...
Factors Affecting Solubility
Carbonation Shrinkage
The concrete's permeability is slightly reduced as calcium carbonate produced during the reaction fills its pores. Furthermore, its strength is slightly enhanced as the water released during the reaction...
Sulfate Attack on Concrete
Sulfates from sources like soil, groundwater, or industrial effluents...
Acid Attack on Concrete
The rate at which hydrogen...