Molecular Weight Controls Interactions between Plastic Deformation and Fracture in Cold Spray of Glassy Polymers
Jeeva Muthulingam1, Anuraag Gangineri Padmanaban2, Nand K Singh1,3
1Department of Mechanical Engineering, Rowan University, Glassboro, New Jersey08028, United States.
Abstract:
Polymer cold spray has gained considerable attention as a novel manufacturing process. A promising aspect of this technology involves the ability to deposit uniform polymer coatings without the requirements of solvent and/or high-temperature conditions. The present study investigates the interplay between shear instability, often considered to be the primary mechanism for bond formation, and fracture, as a secondary energy dissipation mechanism, collectively governing the deposition of glassy thermoplastics on similar and dissimilar substrates. A hybrid experimental-computational approach is utilized to explore the simultaneous effects of several interconnected phenomena, namely the particle-substrate relative deformability, molecular weights, and the resultant yielding versus fracture of polystyrene particles, examined herein as a model material system. The computational investigations are based on constitutive plasticity and damage equations determined and calibrated based on a statistical data mining approach applied to a wide collection of previously reported stress-strain and failure data. Results obtained herein demonstrate that the underlying adhesion mechanisms depend strongly on the molecular weight of the sprayed particles. It is also shown that although the plastic deformation and shear instability are still the primary bond formation mechanisms, the molecular-weight-dependent fracture of the sprayed glassy polymers is also a considerable phenomenon capable of significantly affecting the deposition process, especially in cases involving the cold spray of soft thermoplastics on hard substrates. The strong interplay between molecular-weight-dependent plastic yielding and fracture in the examined system emphasizes the importance of molecular weight as a critical variable in the cold spray of glassy polymers, also highlighting the possibility of process optimization by proper feedstock selection.
More Related Videos
07:37Full-field Strain Measurements for Microstructurally Small Fatigue Crack Propagation Using Digital Image Correlation Method
Published on: January 16, 2019
09:54Author Spotlight: Enhancing Fiber Composite Laminate Quality with the Wet Hand Lay-Up/Vacuum Bag Process
Published on: June 30, 2023
Related Concept Videos
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...
Polymer Classification: Crystallinity
Crystalline domains are the regions where polymer chains are aligned in an orderly manner and held together in proximity by intermolecular forces. For example, chains in the crystalline domains of polyethylene and nylon are bound together by van der Waals...
Polymers: Defining Molecular Weight
The number average molecular weight (Mn) is the summation of the number...
Polymers: Molecular Weight Distribution
Plasticity
Plastic Behavior