Mechanical and Microcrack Evolution Characteristics of Roof Rock of Coal Seam with Different Angle of Defects Based

Qinghai Deng1, Jiaqi Liu1, Junchao Wang2

  • 1College of Earth Science and Engineering, Shandong University of Science and Technology, Qingdao 266590, China.

Related Concept Videos

Microcracking in Concrete01:20

Microcracking in Concrete

Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
173
Types of Non-structural Cracks in Concrete01:28

Types of Non-structural Cracks in Concrete

Non-structural cracks are primarily of three types: plastic, early-age thermal, and drying shrinkage cracks. Plastic cracks are further classified into plastic shrinkage cracks and plastic settlement cracks.
Plastic shrinkage cracks typically form within hours after the concrete is poured. The concrete's surface dries faster than the bottom, creating tensile stress that the still-plastic concrete cannot withstand, leading to diagonal or randomly patterned cracks on the concrete surface.
216
Porosity in Cement Paste01:18

Porosity in Cement Paste

The porosity of concrete is a measure of the void spaces within its structure. These spaces impact its strength and durability significantly. When water and cement interact, a chemical reaction called hydration creates a semi-solid paste. This paste includes combined water, making up approximately 23% of the cement's dry mass, and gel water, which fills minuscule voids known as gel pores, accounting for about 28% of the cement gel volume.
The balance of water to cement in the mix is...
195
Cavity Drainage and Flashings in Masonry walls01:20

Cavity Drainage and Flashings in Masonry walls

Typically, a cavity wall consists of two wythes separated by a gap of at least 2 inches, which may contain insulation while still maintaining a minimum clear space of 1 inch to facilitate adequate drainage. Advanced methods like the insertion of a continuous drainage mat can further reduce this space while ensuring effective moisture expulsion.
Weep holes, strategically placed at the base of the cavity, are critical for draining accumulated water. These openings are created by leaving head...
119
Fatigue01:21

Fatigue

Fatigue occurs when materials rupture under repeated or fluctuating loads, even at stress levels far below their static breaking strength. It typically results in brittle failure, even for ductile materials. It is a critical consideration in designing machines and structural components subjected to repetitive or varying loads. The nature of these loadings can range from fluctuating loads like unbalanced pump impellers causing vibrations to repeatedly bending a thin steel rod wire back and forth...
220
Shear on the Horizontal Face of a Beam Element01:16

Shear on the Horizontal Face of a Beam Element

To understand shear on the flat side of a prismatic beam element, consider the vertical and horizontal shearing forces, and the normal forces, acting on the element. The element's upper (U) and lower (L) sections, which are divided by the beam's neutral axis, are examined. The equilibrium of these forces is determined by applying the equilibrium equation, which helps identify the horizontal shearing force. This force is directly related to the bending moments and the cross-section's...
271