Abstract:
Additively manufactured austenitic stainless steel 316L is composed of a cellular structure, which has a directionality, and is observed with a different morphology depending on the observation direction. The cellular structure morphology that appears with a high probability in grains with a specific grain orientation is determined. Taylor factor, which is calculated by considering grain orientation, is related to cellular structure morphology due to the directional cellular structure in additively manufactured austenitic stainless steel 316L. The Taylor factor affects the mechanical properties. The yield strength of additively manufactured SUS316L can be explained by the correlation between cellular structure morphology, grain orientation, and Taylor factor.
Related Concept Videos
Yield Criteria for Ductile Materials under Plane Stress
The Maximum Shearing Stress Criterion, also known as...
Stress-Strain Diagram - Ductile Materials
Hooke's Law
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...
Relation between Poisson's ratio, Modulus of Elasticity and Modulus of Rigidity
Stress Concentrations