Related Experiment Video
Updated: Aug 7, 2025

Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
Effect of aging and cementation systems on the bond strength to root dentin after fiber post cementation
Caio Henrique de Paula Nogueira1, Mariana Bena Gelio1, João Felipe Besegato1
1Department of Restorative Dentistry, School of Dentistry, Araraquara, São Paulo State University - UNESP, Araraquara, São Paulo, Brazil.
Abstract:
This study evaluated the effect of aging and cementation of fiber posts using glass ionomer and resin cements on push-out bond strength, failure mode, and resin tag formation. One hundred and twenty bovine incisors were used. After post-space preparation, the specimens were randomly allocated into 12 groups (n = 10) according to the cementation system used: GC - GC Gold Label Luting & Lining); RL - RelyX Luting 2; MC - MaxCem Elite; RU - RelyX U200 and the aging periods (24 hours, 6 months, and 12 months). Slices from the cervical, middle, and apical thirds were obtained and analyzed by push-out bond strength test and confocal laser scanning microscopy. One-way ANOVA and Tukey's post-hoc test was used at a significance level of 5%. For the push-out bond strength test, no differences among GC, RU, and MC in the cervical and middle thirds were observed, regardless of the period of storage (P > 0.05). In the apical third, GC and RU showed similar bond strength but higher than other groups (P > 0.05). After 12 months, GC showed the highest bond strength (P < 0.05). Bond strength to post-space dentin decreased over time, regardless of the cementation system used. Cohesive failure was the most frequent, regardless of the period of storage, cementation system, and post-space third. Tag formation was similar among all groups. After 12 months, GC showed the highest bond strength values.
Related Concept Videos
Bonding and Strength of Aggregate
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Strength and Heat of Hydration
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...
Porosity in Cement Paste
The balance of water to cement in the mix is...
Soundness of Cement
Curing of Concrete