Related Experiment Video
Updated: Aug 5, 2025

Author Spotlight: Unraveling the Role of Earthworms in Enhancing Mineral Weathering for CO2 Removal
Published on: November 10, 2023
Quality assessment and quality control of deep soil mixing columns based on a cement-content controlled method
Jinyu Zuo1, Baotian Wang2,3, Wenwei Li1
1Key Laboratory of Ministry of Education for Geomechanics and Embankment Engineering, Hohai University, Nanjing, People's Republic of China.
Abstract:
This paper presents a cement-content controlled method for quality assessment and quality control of the deep soil mixing (DSM) columns in slope reinforcement. The ethylene diamine tetraacetic acid (EDTA) titration method was modified and used for the cement content measurement of core samples, and the effects of curing conditions and curing period on the titration results were investigated. 35 DSM columns with different construction parameters were installed in the test section, and cement content and unconfined compression tests of field core samples were conducted. The relationship between the unconfined compressive strength (UCS) and cement content of DSM columns was formulated, and the quality of DSM columns with different construction parameters was assessed. The test results suggested that the failure strength of the field cores was approximately 15-55% lower than that of laboratory samples with the same cement content. In single columns, the coefficient of variation (CV) of cement content had a negative correlation with the average failure strength and a positive correlation with the coefficient of variation of failure strength. Bidirectional mixing method, lower penetration and withdrawal velocity, more mixing blades and larger number of mixings could improve the uniformity of the DSM columns.
More Related Videos
Related Concept Videos
Mixing Concrete
Testing Water Quality
Measurement of Air Content in Concrete
The pressure method,...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Mixing Time
Slump Test
Concrete is poured into the mold in three layers to conduct the test. Each layer is compacted 25 times with a steel tamping rod, which has a five-eighths-inch diameter and a rounded end, to ensure even distribution and eliminate...