Related Experiment Video
Updated: Aug 5, 2025

Fabrication of Large-area Free-standing Ultrathin Polymer Films
Published on: June 3, 2015
Synthesis of Wrinkle-Free Metallic Thin Films in Polymer by Interfacial Instability Suppression with Nanoparticles
Maryam Jalali-Mousavi1, Samuel Kok Suen Cheng1, Jian Sheng1
1College of Engineering, Texas A&M University-Corpus Christi, Corpus Christi, TX 78412, USA.
Abstract:
Synthesis of a smooth conductive film over an elastomer is vital to the development of flexible optics and wearable electronics, but applications are hindered by wrinkles and cracks in the film. To date, a large-scale wrinkle-free film in an elastomer has yet to be achieved. We present a robust method to fabricate wrinkle-free, stress-free, and optically smooth thin film in elastomer. Targeting underlying mechanisms, we applied nanoparticles between the film and elastomer to jam the interface and subsequently suppress interfacial instabilities to prevent the formation of wrinkles. Using polydimethylsiloxane (PDMS) and parylene-C as a model system, we have synthesized large-scale (>10 cm) wrinkle-free Al film over/in PDMS and demonstrated the principle of interface jamming by nanoparticles. We varied the jammer layer thickness to show that, as the layer exceeds a critical thickness (e.g., 150 nm), wrinkles are successfully suppressed. Nano-indentation experiments revealed that the interface becomes more elastic and less viscoelastic with respect to the jammer thickness, which further supports our assertion of the wrinkle suppression mechanism. Since the film was embedded in a polymer matrix, the resultant film was highly deformable, elastic, and optically smooth with applications for deformable optical sensors and actuators.