Related Experiment Video
Updated: Aug 5, 2025

Author Spotlight: Advancing 3D Coculture Systems with PVA-PCL Nanofibrous Membranes
Published on: December 27, 2024
Development and Characterization of Drug Loaded PVA/PCL Fibres for Wound Dressing Applications
Ali Afzal1, Mohammed Jalalah2,3, Abid Noor4
1Department of Textile Engineering, School of Engineering & Technology, National Textile University, Faisalabad 37610, Pakistan.
Abstract:
Nowadays, synthetic polymers are used in medical applications due to their special biodegradable, biocompatible, hydrophilic, and non-toxic properties. The materials, which can be used for wound dressing fabrication with controlled drug release profile, are the need of the time. The main aim of this study was to develop and characterize polyvinyl alcohol/polycaprolactone (PVA/PCL) fibres containing a model drug. A dope solution comprising PVA/PCL with the drug was extruded into a coagulation bath and became solidified. The developed PVA/PCL fibres were then rinsed and dried. These fibres were tested for Fourier transform infrared spectroscopy, linear density, topographic analysis, tensile properties, liquid absorption, swelling behaviour, degradation, antimicrobial activity, and drug release profile for improved and better healing of the wound. From the results, it was concluded that PVA/PCL fibres containing a model drug can be produced by using the wet spinning technique and have respectable tensile properties; adequate liquid absorption, swelling %, and degradation %; and good antimicrobial activity with the controlled drug release profile of the model drug for wound dressing applications.