Effect of Ru on Deformation Mechanism and Microstructure Evolution of Single-Crystal Superalloys under
Stephen Okhiai Emokpaire1,2, Nan Wang1,3, Jide Liu1
1Shi-Changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China.
Abstract:
In this work, the effect of the Ru element on the γ'-phase evolution and deformation mechanism in the fourth-generation Ni-based single-crystal superalloy was investigated. Results show that the Ru element alters the distribution coefficient of other elements in the alloy to produce reverse partitioning behavior, which leads to a difference in microstructure between 0Ru and 3Ru. The addition of Ru triggered the incubation period before the beginning of the primary creep stage, which depends on the creep temperature and stress during creep deformation. TEM results revealed that Ru addition inhibits the slip system {111}<112> at medium-temperature (760-1050 °C) and high-stress (270-810 MPa) creep, which brings a considerably low creep rate and high creep life to the Ru-containing alloy.
More Related Videos
Related Concept Videos
Stress-Strain Diagram - Ductile Materials
Effects of Creep
Temperature Dependent Deformation
Creep in Concrete
Plastic Behavior
Residual Stresses