Related Experiment Video
Updated: Aug 3, 2025

Isolation of Native Soil Microorganisms with Potential for Breaking Down Biodegradable Plastic Mulch Films Used in Agriculture
Published on: May 10, 2013
Moisture Sorption Isotherms and Thermodynamic Properties of Biodegradable Polymers for Application in Food Packaging
Loleny Tavares1,2,3, Liliana R Sousa1,2,3, Sara Magalhães da Silva1,2,3
1School of Design, Management and Production Technologies Northern Aveiro, University of Aveiro, Estrada do Cercal, 449, 3720-509 Oliveira de Azeméis, Portugal.
Abstract:
This work aims to evaluate the influence of two starch-based materials (B16 and B20) on the moisture sorption isotherms, determined at 30, 40, and 50 °C, where B16 contains 5% (w/w) more starch than B20. Thermodynamic functions (differential enthalpy (∆Hdif), differential entropy (∆Sdif), integral enthalpy (Δhint), integral entropy (ΔSint), free Gibbs energy (∆G), and spreading pressure (φ)) were used to understand the water-binding behaviors and the energy requirements to remove the moisture content from the surface of these materials. The moisture sorption isotherms exhibited type III behavior, and the Guggenheim-Anderson-de Boer (GAB) model was the most suitable to fit the experimental moisture adsorption data. The adsorption isotherms of microparticles were enthalpy-controlled, with isokinetic temperature values of 221.45 and 279.77 K for B16 and B20, respectively, being higher than the harmonic mean temperature (312.94 K). The values of ∆G were positive (45.274 and 44.307 kJmol-1 for B16 and B20, respectively), indicating a non-spontaneous process. The spreading pressure values increased with increasing water activity (aw) for all isotherms. Higher values of ∆Hdif and ∆Sdif obtained from B16 confirmed its higher number of sorption sites available for binding with water molecules when compared to B20, making it less suitable for application in the food packaging industry.
Related Concept Videos
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the...
Polymer Classification: Architecture
Moisture Content and Bulking of Aggregate
When aggregates are exposed to rain or sit in stockpiles, they absorb moisture, which must be...