Effect of polybutylene adipate terephthalate on the properties of starch/polybutylene adipate terephthalate shape
Zhaomeng Long1, Wenjun Wang1, Yue Zhou1
1School of Materials Science and Engineering, Zhejiang Sci-Tech University, Hangzhou, Zhejiang 310018, China.
Abstract:
In this work, the starch/polybutylene adipate terephthalate (PBAT) composite films with high starch content were prepared by hot-pressing and ultraviolet cross-linking methods using cassava starch, benzophenone (BP), degradable PBAT and citric acid as film-forming substrate, photosensitizer, toughening material and solvent, respectively. The results showed that starch and PBAT had excellent performance, resulting in the composites films exhibit robust tensile strength (9.90 MPa), decent elongation at break (500.05 %) and excellent shape memory property. Under 30 % pre-tensile strain, the shape memory fixity and recovery ratios reached 96.58 % and 93.94 %, respectively. In addition, the starch-based films were successfully rendered hydrophobic by PBAT hydrophobic characteristics. PBAT not only secures the biodegradability of the starch/PBAT composites films, but also improves the mechanical properties of them, and meets the requirements of the thermal shrinkage films when subjected to large strain.
More Related Videos
Related Concept Videos
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the...
Polymer Classification: Stereospecificity
Polymer Classification: Architecture
Plastic Behavior
Polymer Classification: Crystallinity
Crystalline domains are the regions where polymer chains are aligned in an orderly manner and held together in proximity by intermolecular forces. For example, chains in the crystalline domains of polyethylene and nylon are bound together by van der Waals...
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...