Related Experiment Video
Updated: Jul 31, 2025

Processing of Bulk Nanocrystalline Metals at the US Army Research Laboratory
Published on: March 7, 2018
Experimental investigation and multi-objective optimization of eco-friendly near-dry electrical discharge machining
Nagarajan Vasantha Gowri1, Jaiprakash Narain Dwivedi2, Kondreddi Krishnaveni1
1Department of Electrical and Electronics Engineering, Chaitanya Bharathi Institute of Technology, Hyderabad, Telangana, 500075, India.
Abstract:
The near-dry electrical discharge machining processes have been conducted using air-mist or gas mist as a dielectric fluid to minimize the environmental impacts. In this article, near-dry electrical discharge machining (NDEDM) experiments have been performed to improve machining performance using an oxygen-mist dielectric fluid, a copper composite electrode, and Cu-Al-Be polycrystalline shape memory alloy (SMA) work materials. The copper composite electrode is made up of 12 wt% silicon carbide and 9 wt% graphite particles. The oxygen-mist pressure (Op), pulse on time (Ton), spark current (Ip), gap voltage (Gv), and flow rate of mixed water (Fr) were used as process parameters, and the material removal rate (MRR), tool wear rate (TWR), and surface roughness (SR) were used as performance characteristics. The global optimal alternative solution has been predicted by the PROMETHEE-II (Preference Ranking Organization METhod for Enrichment Evaluations-II) optimization technique. The best combinations of process parameters have been used to examine the microstructure of composite tools and SMA-machined surfaces by scanning electron microscopy (SEM) analysis. The best global optimum settings (oP: 9 bar, Ip: 60 µs, Ip: 12 A, Gv: 40 V, and Fr: 12 ml/min) are predicted to attain optimum machining performance (MRR: 39.049 g/min, TWR: 1.586 g/min, and SR: 1.78 µm). The tool wear rate of the NDEDM process has been significantly reduced by the copper composite electrode due to increasing microhardness, wear resistance, and melting point. When compared to the pure copper electrode tool, the MRR of NDEDM is improved to 21.91%, while the TWR and SR are reduced to 46.66% and 35.02%, respectively.