From Electronic Waste to 3D-Printed Product, How Multiple Recycling Affects High-Impact Polystyrene (HIPS) Filament
Edbert Wing Hanitio1, Novan Rifky Lutfhyansyah1, Balqis Mentari Efendi1
1Materials Science and Engineering Research Group, Faculty of Mechanical and Aerospace Engineering, Institut Teknologi Bandung, Jl. Ganesha No. 10, Bandung 40132, Indonesia.
Abstract:
The rapid growth of the electronics industry is producing excessive electronic waste. One of the common types of materials in electronic waste is high-impact polystyrene (HIPS). In this study, HIPS from electronic waste was recycled through an extrusion process and used as a 3D print filament. The effects of recycling on printability, physical properties, and mechanical properties in horizontal and vertical directions were examined. It was found that until the fourth-cycle, mechanical properties such as horizontal tensile strength, horizontal flexural strength, vertical flexural strength, and vertical impact strength were comparable with virgin commercial filament. In addition, the vertical flexural modulus in the fourth cycle increased by 77.28%. However, the density of recycled HIPs' first to the fourth cycle slightly decreased by 10.6%, and the melt flow rate increased by 20.3%. It was also observed that until the third cycle, the effect of the reprocessing steps was insignificant on the defect of the 3D-printed product. In general, the experiments show various results, mainly in mechanical properties. Nevertheless, recycled HIPS filaments are comparable to or better than commercial ones in some cases. As a result, recycled HIPS filaments hold the potential to be considered as an alternative to other types of 3D print filaments.
Related Concept Videos
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the...
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...
Polymer Classification: Stereospecificity
Polymer Classification: Architecture