Experimental Study on Ultrasonic Assisted Turning of GH4068 Superalloy

Renke Kang1, Pengnan Zhang1, Zhaocheng Wei1

  • 1State Key Laboratory of High-Performance Precision Manufacturing, School of Mechanical Engineering, Dalian University of Technology, Dalian 116014, China.