Research on Determining Elastic-Plastic Constitutive Parameters of Materials from Load Depth Curves Based on

Zhentao Li1, Yun Ye2, Guanjun Zhang1

  • 1State Key Laboratory of Advanced Design and Manufacturing for Vehicle Body, Hunan University, Changsha 410082, China.

Micromachines
|May 27, 2023
PubMed

Related Concept Videos

Plastic Behavior01:21

Plastic Behavior

A material's elastic behavior is characterized by the disappearance of stress once the load is removed, allowing the material to return to its original state. However, when stress surpasses the yield point, yielding commences, marking the onset of plastic deformation or permanent set. This change from elastic to plastic behavior is influenced by the peak stress value and the duration before the load is removed. An intriguing observation occurs when a specimen is loaded, unloaded, and...
232
Residual Stresses in Bending01:18

Residual Stresses in Bending

In the study of elastoplastic members subjected to bending moments, understanding the loading and unloading phases is crucial for assessing material behavior and structural integrity. During the loading phase, as the bending moment increases, the material initially responds elastically, adhering to Hooke's Law, where stress is directly proportional to strain. When the load exceeds the yield strength, plastic deformation occurs, resulting in permanent strain and deformation that remains even...
214
Members Made of Elastoplastic Material01:19

Members Made of Elastoplastic Material

The behavior of elastoplastic materials under bending stresses, particularly in structural members with rectangular cross-sections, is crucial for predicting material responses and understanding failure modes. Initially, when a bending moment is applied, the stress distribution across the section follows Hooke's Law and is linear and elastic. This distribution means the stress increases from the neutral axis to the maximum at the outer fibers, up to the elastic limit.
As the bending moment...
126
Elasticity in Concrete01:20

Elasticity in Concrete

Upon subjecting concrete to moderate or high uniaxial compressive or tensile stresses, the strain response is non-linear relative to the stress applied. As the stress is removed, the resulting stress-strain curve deviates from the original path traced during loading, creating a hysteresis loop, indicative of the concrete's non-linear and non-elastic properties. Typically, a material's modulus of elasticity, which is a measure of the material's stiffness, is inferred from the linear...
120
Hooke's Law01:26

Hooke's Law

Hooke's law, a pivotal principle in material science, establishes that the strain a material undergoes is directly proportional to the applied stress, defined by a factor called the modulus of elasticity or Young's modulus.
488
Stress-Strain Diagram - Ductile Materials01:24

Stress-Strain Diagram - Ductile Materials

The stress-strain relationship in ductile materials such as structural steel or aluminium is intricate and progresses through several stages. When a specimen is loaded, it initially exhibits a linear length increase, depicted by a steep straight line on the stress-strain diagram. It indicates the material is elastically deforming and will return to its original shape once unloaded. However, when a critical stress value is reached, plastic deformation begins. This stage sees substantial...
877