Understanding capacity fade in organic redox-flow batteries by combining spectroscopy with statistical inference techniques
Related Experiment Video
Updated: Jul 26, 2025

A Protocol for Electrochemical Evaluations and State of Charge Diagnostics of a Symmetric Organic Redox Flow Battery
Published on: February 13, 2017
Sanat Vibhas Modak1, Wanggang Shen1, Siddhant Singh1
1Department of Mechanical Engineering, University of Michigan, Ann Arbor, MI, 48109, USA.
Abstract:
Organic redox-active molecules are attractive as redox-flow battery (RFB) reactants because of their low anticipated costs and widely tunable properties. Unfortunately, many lab-scale flow cells experience rapid material degradation (from chemical and electrochemical decay mechanisms) and capacity fade during cycling (>0.1%/day) hindering their commercial deployment. In this work, we combine ultraviolet-visible spectrophotometry and statistical inference techniques to elucidate the Michael attack decay mechanism for 4,5-dihydroxy-1,3-benzenedisulfonic acid (BQDS), a once-promising positive electrolyte reactant for aqueous organic redox-flow batteries. We use Bayesian inference and multivariate curve resolution on the spectroscopic data to derive uncertainty-quantified reaction orders and rates for Michael attack, estimate the spectra of intermediate species and establish a quantitative connection between molecular decay and capacity fade. Our work illustrates the promise of using statistical inference to elucidate chemical and electrochemical mechanisms of capacity fade in organic redox-flow battery together with uncertainty quantification, in flow cell-based electrochemical systems.
More Related Videos
07:55Elemental-sensitive Detection of the Chemistry in Batteries through Soft X-ray Absorption Spectroscopy and Resonant Inelastic X-ray Scattering
Published on: April 17, 2018
08:41Electrochemical Impedance Spectroscopy as a Tool for Electrochemical Rate Constant Estimation
Published on: October 10, 2018
Related Concept Videos
Voltammetry: Factors Affecting Measurements
Redox Equilibria: Overview
Redox Titration: Overview
Voltammetry: Overview
A voltammetric cell uses three electrodes: a working electrode, a reference electrode, and an auxiliary electrode. The redox reactions occur in the working...
Electrolysis
Energy Stored in Capacitors
By integrating the equation that relates voltage and current in a capacitor, one can derive an equation for the voltage across the capacitor at any given time. This equation is crucial in understanding and predicting the behavior of capacitors in...