Related Experiment Video
Updated: Jul 23, 2025

Characterization of Electrode Materials for Lithium Ion and Sodium Ion Batteries Using Synchrotron Radiation Techniques
Published on: November 11, 2013
Polydopamine Derived NaTi2(PO4)3-Carbon Core-Shell Nanostructures for Aqueous Batteries and Deionization Cells
Nadežda Traškina1, Gintarė Gečė1, Jurgis Pilipavičius1,2
1Center for Physical Sciences and Technology (FTMC), Saulėtekio al. 3, Vilnius LT-10257, Lithuania.
Abstract:
Due to their stability and structural freedom, NASICON-structured materials such as NaTi2(PO4)3 show a lot of promise as active electrode materials for aqueous batteries and deionization cells. However, due to their low intrinsic electronic conductivity, they must usually be composited with carbon to form suitable electrodes for power applications. In this work, two series of NaTi2(PO4)3-carbon composite structures were successfully prepared by different approaches: postsynthetic pyrolytic treatment of citric acid and surface polymerized dopamine. The latter route allows for a superior carbon loading control and yields more uniform and continuous particle coatings. The homogeneity of the polydopamine derived core-shell carbon layer is supported by FTIR, TEM, and XPS analysis. Combustion elemental analysis also indicates significant nitrogen doping in the final carbonaceous structure. The galvanostatic charge and discharge cycling results show similar initial capacities and their retention, but at only half of the carbon loading in polydopamine derived samples. The overall results indicate that careful nanostructure engineering could yield materials with superior properties and stability suitable for various electrochemical applications such as aqueous Na-ion batteries and deionization cells.
More Related Videos
07:58Bio-inspired Polydopamine Surface Modification of Nanodiamonds and Its Reduction of Silver Nanoparticles
Published on: November 14, 2018
10:27Simultaneous Multi-surface Anodizations and Stair-like Reverse Biases Detachment of Anodic Aluminum Oxides in Sulfuric and Oxalic Acid Electrolyte
Published on: October 5, 2017