Unveiling orientation dependence of anisotropic plasticity in polycrystalline copper by nanoindentation

Rongkai Tan1, Zhanfeng Wang1,2, Shilei Wu3

  • 1Key Laboratory of Conveyance Equipment (East China Jiaotong University), Ministry of Education, Nanchang 330013, People's Republic of China.

Nanotechnology
|August 16, 2023
PubMed

Related Concept Videos

Plastic Behavior01:21

Plastic Behavior

A material's elastic behavior is characterized by the disappearance of stress once the load is removed, allowing the material to return to its original state. However, when stress surpasses the yield point, yielding commences, marking the onset of plastic deformation or permanent set. This change from elastic to plastic behavior is influenced by the peak stress value and the duration before the load is removed. An intriguing observation occurs when a specimen is loaded, unloaded, and...
222
Plasticity00:58

Plasticity

Plasticity is the property where an object loses its elasticity and undergoes irreversible deformation, even after the deformation forces are eliminated. If a material deforms irreversibly without increasing stress or load, then this is called ideal plasticity. For example, when a force is applied to an aluminum rod, it changes its shape, but it does not return to its original shape once the force is removed. Plastic deformation or ductility is thus a permanent deformation or change in the...
2.2K
Relation between Poisson's ratio, Modulus of Elasticity and Modulus of Rigidity01:15

Relation between Poisson's ratio, Modulus of Elasticity and Modulus of Rigidity

Deformation occurs in axial and transverse directions when an axial load is applied to a slender bar. This deformation impacts the cubic element within the bar, transforming it into either a rectangular parallelepiped or a rhombus, contingent on its orientation. This transformation process induces shearing strain. Axial loading elicits both shearing and normal strains. Applying an axial load instigates equal normal and shearing stresses on elements oriented at a 45° angle to the load axis.
291
Plastic Deformations01:14

Plastic Deformations

It is essential to understand how structural members behave under plastic deformation when the bending stress exceeds the material's yield strength. This state of deformation permanently alters the shape of the member, in contrast to the linear elastic behavior observed before yielding. The strain at any point in the member is expressed in terms of maximum strain. Notably, the neutral axis, which coincides with the centroid during elastic bending, shifts away from the centroid under plastic...
109
Generalized Hooke's Law01:22

Generalized Hooke's Law

The generalized Hooke's Law is a broadened version of Hooke's Law, which extends to all types of stress and in every direction. Consider an isotropic material shaped into a cube subjected to multiaxial loading. In this scenario, normal stresses are exerted along the three coordinate axes. As a result of these stresses, the cubic shape deforms into a rectangular parallelepiped. Despite this deformation, the new shape maintains equal sides, and there is a normal strain in the direction of the...
1.1K
Hooke's Law01:26

Hooke's Law

Hooke's law, a pivotal principle in material science, establishes that the strain a material undergoes is directly proportional to the applied stress, defined by a factor called the modulus of elasticity or Young's modulus.
469