Related Experiment Video
Updated: Jul 17, 2025

Zinc-Sponge Battery Electrodes that Suppress Dendrites
Published on: September 29, 2020
Alkaline Ni-Zn Rechargeable Batteries for Sustainable Energy Storage: Battery Components, Deterioration Mechanisms,
Katerina Bogomolov1, Yair Ein-Eli1,2
1Department of Materials Science and Engineering, Technion - Israel Institute of Technology, Haifa, 3200003, Israel.
Abstract:
The demand for long-term, sustainable, and low-cost battery energy storage systems with high power delivery capabilities for stationary grid-scale energy storage, as well as the necessity for safe lithium-ion battery alternatives, has renewed interest in aqueous zinc-based rechargeable batteries. The alkaline Ni-Zn rechargeable battery chemistry was identified as a promising technology for sustainable energy storage applications, albeit a considerable investment in academic research, it still fails to deliver the requisite performance. It is hampered by a relatively short-term electrode degradation, resulting in a decreased cycle life. Dendrite formation, parasitic hydrogen evolution, corrosion, passivation, and dynamic morphological growth are all challenging and interrelated possible degradation processes. This review elaborates on the components of Ni-Zn batteries and their deterioration mechanisms, focusing on the influence of electrolyte additives as a cost-effective, simple, yet versatile approach for regulating these phenomena and extending the battery cycle life. Even though a great deal of effort has been dedicated to this subject, the challenges remain. This highlights that a breakthrough is to be expected, but it will necessitate not only an experimental approach, but also a theoretical and computational one, including artificial intelligence (AI) and machine learning (ML).
More Related Videos
07:55Elemental-sensitive Detection of the Chemistry in Batteries through Soft X-ray Absorption Spectroscopy and Resonant Inelastic X-ray Scattering
Published on: April 17, 2018
10:41The Effect of Charging and Discharging Lithium Iron Phosphate-graphite Cells at Different Temperatures on Degradation
Published on: July 18, 2018
Related Concept Videos
Batteries and Fuel Cells
Voltaic/Galvanic Cells
Spontaneous redox reactions occur abundantly in nature. The chemical reaction occurring in a disposable AA battery powering our remote controls is one such example of a spontaneous redox reaction. Another example is the immersion of coiled copper wire into an aqueous silver nitrate solution. The reaction shows a gradual, visually impressive color change from colorless to bright blue and the formation of a grey precipitate on the copper wire. In this experiment,...
The Nernst Equation
The interconnection between standard cell potentials and various thermodynamic parameters such as the standard free energy change ΔG° and equilibrium constant K has been previously explored. For example, a redox reaction involving zinc(II) and tin(II) ions at 1 M concentration with Eºcell = +0.291 V and ΔG° = −56.2 kJ is spontaneous.
Electrolysis
Balancing Redox Equations