Related Experiment Video
Updated: Jun 29, 2026

Scale-up Chemical Synthesis of Thermally-activated Delayed Fluorescence Emitters Based on the Dibenzothiophene-S,S-Dioxide Core
Published on: October 24, 2017
High-performance blue OLED using multiresonance thermally activated delayed fluorescence host materials containing
Dongmin Park1, Seokwoo Kang2, Chi Hyun Ryoo1
1Center for Supramolecular Optoelectronic Materials (CSOM), Department of Materials Science and Engineering, Seoul National University, 1 Gwanak-ro, Gwanak-gu, Seoul, 08826, Republic of Korea.
Abstract:
We report three highly efficient multiresonance thermally activated delayed fluorescence blue-emitter host materials that include 5,9-dioxa-13b-boranaphtho[3,2,1-de]anthracene (DOBNA) and tetraphenylsilyl groups. The host materials doped with the conventional N7,N7,N13,N13,5,9,11,15-octaphenyl-5,9,11,15-tetrahydro-5,9,11,15-tetraaza-19b,20b-diboradinaphtho[3,2,1-de:1',2',3'-jk]pentacene-7,13-diamine (ν-DABNA) blue emitter exhibit a high photoluminescence quantum yield greater than 0.82, a high horizontal orientation greater than 88%, and a short photoluminescence decay time of 0.96-1.93 μs. Among devices fabricated using six synthesized compounds, the device with (4-(2,12-di-tert-butyl-5,9-dioxa-13b-boranaphtho[3,2,1-de]anthracen-7-yl)phenyl)triphenylsilane (TDBA-Si) shows high external quantum efficiency values of 36.2/35.0/31.3% at maximum luminance/500 cd m-2/1,000 cd m-2. This high performance is attributed to fast energy transfer from the host to the dopant. Other factors possibly contributing to the high performance are a T1 excited-state contribution, inhibition of aggregation by the bulky tetraphenylsilyl groups, high horizontal orientation, and high thermal stability. We achieve a high efficiency greater than 30% and a small roll-off value of 4.9% at 1,000 cd m-2 using the TDBA-Si host material.