Related Experiment Video
Updated: Jul 15, 2025

Electrospray Deposition of Uniform Thickness Ge23Sb7S70 and As40S60 Chalcogenide Glass Films
Published on: August 19, 2016
Solution processed multi-layered thin films of Ge20Sb5S75 and Ge20Sb5Se75 chalcogenide glasses
Jiri Jemelka1, Karel Palka2,3, Petr Janicek4,5
1Department of General and Inorganic Chemistry, Faculty of Chemical Technology, University of Pardubice, Studentska 95, 53210, Pardubice, Czech Republic.
Abstract:
Solution processed non-toxic Ge20Sb5Se75 chalcogenide glass thin films were deposited using spin-coating method from n-propylamine-methanol solvent mixture in specular optical quality. Optical properties, composition, structure, and chemical resistance were studied in dependence on the annealing temperature. Significant increase of refractive index and chemical resistance caused by thermoinduced structural polymerization and release of organic residua were observed. The high chemical resistance of hard-baked thin films allowed repeated direct depositions by spin-coating, increasing total thickness. Multilayered thin films of amorphous Ge20Sb5Se75 and Ge20Sb5S75 were also successfully prepared by direct deposition for the first time. Solution based deposition of non-toxic Ge20Sb5Se75 thin films in specular optical quality significantly widens the applicability of solution processed chalcogenide glass thin films. Moreover, solution based direct deposition of different glasses on hard-baked thin films opens the way to simple and cost-effective preparation of more sophisticated optical elements (e.g. beam splitters, photonic mirrors).
More Related Videos
06:57Theoretical Calculation and Experimental Verification for Dislocation Reduction in Germanium Epitaxial Layers with Semicylindrical Voids on Silicon
Published on: July 17, 2020
12:21Close-Space Sublimation-Deposited Ultra-Thin CdSeTe/CdTe Solar Cells for Enhanced Short-Circuit Current Density and Photoluminescence
Published on: March 6, 2020