Characterization of hardness and elastic modulus using nanoindentation and correlation with wear behavior of UHMWPE during uniaxial tension
Related Experiment Video
Updated: Jul 14, 2025

Experimental and Data Analysis Workflow for Soft Matter Nanoindentation
Published on: January 18, 2022
Sahitya Movva1, Reeshemah K Burrell2, Hamid Garmestani3
1School of Materials Science and Engineering, Georgia Institute of Technology, Atlanta, GA, 30332, USA; Intel Corporation, 2501 NE Century Blvd, Hillsboro, OR, 97124, USA.
Abstract:
UHMWPE is the material of choice for bearing surfaces in total joint arthroplasty making its wear and mechanical properties important factors of contribution in longevity of prosthetic hip/knee implants. In this study, the variation of hardness and elastic modulus with applied load in textured UHMWPE has been investigated. Texture has been induced through uniaxial tension of UHMWPE modifying its microstructure which in turn influences the wear resistance and hence the mechanical properties of the material. Previous studies have shown hardness to be a major factor influencing wear resistance. However, recently, the ratio of hardness (H) to elastic modulus (E) has been recognized as a more influential parameter of wear resistance. The validity of predicting wear resistance using H/E ratio has been examined in this work. Power law variation with load for the bioimplant material UHMWPE has been investigated at different strain levels. It has been observed that power law exponent of 2 can only be achieved at higher load levels. Overall, this work provides an insight into influencing the properties of bioimplant material UHMWPE by modifying the microstructure of the material through inducing texture which ultimately affects the longevity of the prosthetic implants.
Related Concept Videos
Elasticity in Concrete
Plastic Behavior
Hooke's Law
Strain and Elastic Modulus
Relation between Poisson's ratio, Modulus of Elasticity and Modulus of Rigidity
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used...