Research on Fatigue-Healing Performance of Asphalt Mixture Based on the Semicircular Bending Test
Lijun Wang1, Peifeng Cheng1, Qiang Zhao1
1School of Civil Engineering and Transportation, Northeast Forestry University, Harbin 150040, China.
Abstract:
In order to study the self-healing performance of macroscopic fractures of asphalt mixtures, semicircular bending (SCB) tests were used to test 90# base asphalt mixtures, SBS (Styrene-Butadiene-Styrene) modified asphalt mixtures, and SBS + CR (Chloroprene Rubber) composite modified asphalt mixtures. The F-H-F (the asphalt mixture specimen was fatigued for a certain number of times, then healed under certain conditions, and then fatigued until destroyed) test was carried out, and the fatigue life recovery rate of the fatigue test before and after healing was defined as the healing index (HI). The gray correlation analysis method was used to judge the influence degree of influencing factors on fatigue-healing according to the correlation index. The results show the type of asphalt has the most significant influence on the healing ability of the asphalt mixture. In the case of complete healing, the fatigue-healing performance of the SBS + CR composite modified asphalt mixture was the best, followed by the SBS-modified asphalt mixture, and 90# base asphalt. When the healing temperature is close to the softening point of asphalt, the healing performance of 90# base asphalt is better when the healing temperature is low. When the healing time is longer, the healing performance is better, and there is an optimal healing time. The healing index decreased with the increase in the degree of damage. When the degree of damage is too large, the asphalt mixture will be difficult to heal.
Related Concept Videos
Fatigue Strength of Concrete
Fatigue
Toughness and Hardness of Aggregate
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Vebe Test
To conduct the test, concrete is placed into the slump cone. The concrete is filled in layers and...