Laser-induced immobilization of an amorphous iron-phosphate/Fe3O4 composite on nickel foam for efficient water
Yan Zou1, Man Jin1, Dongdong Zhu1
1School of Chemistry and Materials Science, Institute of Advanced Materials and Flexible Electronics (IAMFE), Nanjing University of Information Science and Technology, 219 Ningliu Road, Nanjing 210044, P. R. China. tangyujia@nuist.edu.cn.
Abstract:
A laser-induced immobilization strategy is applied to prepare an amorphous iron-phosphate/Fe3O4 (L-FePO) composite on a nickel foam (NF) support. By laser-irradiating an iron hydrogen phosphate (FeHP) precursor, a melting and oxidation process leads to the generation of L-FePO with hierarchical pores and an amorphous structure. L-FePO shows exceptional electrocatalytic performance for the OER in an alkaline electrolyte, demonstrating an overpotential of 256 mV at 100 mA cm-2, a Tafel slope of 71 mV dec-1, and good stability over 100 h. The active Fe3O4, partially dissolved phosphate, and newly formed FeOOH species provide abundant active sites, contributing to the excellent OER performance.
Related Concept Videos
Corrosion
Coagulation
Acid Mine Drainage