The combined effect of cohesion and finite size on the collapse of wet granular columns

Yisong Wu1, Yinghao Sun1, Dengming Wang1

  • 1Department of Mechanics and Engineering Science, School of Civil Engineering and Mechanics, and Key Laboratory of Mechanics on Disaster and Environment in Western China, Ministry of Education of China, Lanzhou University, Lanzhou 730000, China. dmwang@lzu.edu.cn.

Soft Matter
|December 5, 2023
PubMed

Related Concept Videos

Cohesion01:07

Cohesion

Cohesion is the attraction between molecules of the same type, such as water molecules. Water molecules have an overall neutral charge but are polar molecule. An oxygen atom in one water molecule has a partial negative charge that can bind to a hydrogen atom with a partial positive charge in a second water molecule, forming a hydrogen bond. Each water molecule can form up to four hydrogen bonds with other water molecules. Hydrogen bonds are responsible for water's cohesive nature.
On a...
54.3K
Design of Columns under a Centric Load01:17

Design of Columns under a Centric Load

The design of columns under centric load is a fundamental aspect of structural engineering and is critical for ensuring the stability and integrity of structures. Euler's and Secant's formulas are central to understanding and calculating the critical load and deformation behaviors of columns, providing a basis for safe and effective structural design.
Euler's formula is applicable under the assumption that the column is a perfect, straight, homogenous prism, and it is operating...
119
Euler's Formula for Pin-Ended Columns01:21

Euler's Formula for Pin-Ended Columns

In structural engineering, the stability of columns under compressive axial loads is a critical consideration, described as buckling. A typical example involves a column PQ, which is pin-connected at both ends and subjected to a centric axial load F applied at one end, with a reaction force of F' = -F at the other end. Here, it is crucial to understand that when an applied load exceeds the critical load, buckling occurs as the system becomes unstable.
To calculate the critical load,...
323
Behavior of Concrete Under Compressive Load01:23

Behavior of Concrete Under Compressive Load

Concrete exhibits specific behaviors under different compressive loads. Understanding this is crucial for understanding its structural integrity. When concrete undergoes uniaxial compression, it tends to develop cracks that run parallel to the direction of the force. These parallel cracks stem from localized tensile stresses that occur perpendicular to the compression direction. Additionally, angled cracks may appear due to the formation of shear planes.
As the concrete specimen fractures under...
175
Euler's Formula to Columns with Other End Conditions01:15

Euler's Formula to Columns with Other End Conditions

Euler's formula is very important in the field of structural engineering, providing a foundation for understanding the critical loading conditions of pin-ended columns. This formula links the modulus of elasticity, the moment of inertia of the cross-section, and the column's length, offering a precise calculation of the critical load at which a column is prone to buckling.
529
Tensile Strength Considerations of Concrete01:16

Tensile Strength Considerations of Concrete

Considering the tensile strength of concrete involves recognizing that the theoretical strength of cement paste can be up to a thousand times higher than what is observed in practical applications. This significant discrepancy is largely attributed to the presence of microscopic cracks within the concrete. These cracks tend to amplify stress at their tips when a load is applied, a phenomenon explained by Griffith's theory of brittle fracture.
The dimensions and shape of a concrete specimen...
132