Related Experiment Video
Updated: Jul 9, 2025

Two-way Valorization of Blast Furnace Slag: Synthesis of Precipitated Calcium Carbonate and Zeolitic Heavy Metal Adsorbent
Published on: February 21, 2017
Carbonation of a Synthetic CAF Compound by CO2 Absorption and Its Effect on Cement Matrix
Woong-Geol Lee1, Seung-Min Kang2, Myong-Shin Song1
1Research Center of Advanced Convergence Processing on Materials, Kangwon National University, Samcheok 25913, Republic of Korea.
Abstract:
In the field of construction materials, the development of fundamental technologies to reduce energy consumption and CO2 emissions, such as manufacturing process improvement and the expanded use of alternative materials, is required. Technologies for effectively reducing energy consumption and improving CO2 absorption and reduction that can meet domestic greenhouse gas reduction targets are also required. In this study, calcium-aluminate-ferrite (CAF), a ternary system of CaO·Al2O3·Fe2O3, was sintered at a low temperature (1100 °C) to examine the possibility of CO2 adsorption, and excellent CO2 absorption performance was confirmed, as the calcite content was found to be 11.01% after 3 h of the reaction between synthetic CAF (SCAF) and CO2. In addition, the physical and carbonation characteristics were investigated with respect to the SCAF substitution rate for cement (10%, 30%, 50%, 70%, and 100%). It was found that SCAF 10% developed a compressive strength similar to that of ordinary Portland cement (OPC 100%), but the compressive strength tended to decrease as the SCAF substitution rate increased. An increase in the SCAF substitution rate led to the rapid penetration of CO2, and carbonation was observed in all the specimens after 7 days. As carbonation time increased, the CO2 diffusion coefficient tended to decrease. This is because the diffusion of CO2 in the cement matrix follows the semi-infinite model of Fick's second law. SCAF can contribute to reduced energy consumption and CO2 emissions because of the low-temperature sintering and can absorb and fix CO2 when a certain amount is substituted.
Related Concept Videos
Carbonation Shrinkage
The concrete's permeability is slightly reduced as calcium carbonate produced during the reaction fills its pores. Furthermore, its strength is slightly enhanced as the water released during the reaction...
Hydration of Cement
Acid Attack on Concrete
The rate at which hydrogen...
Strength and Heat of Hydration
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...
Additives and Fillers in Concrete
The...
Factors Affecting Solubility