Abstract:
Warp sizing is a key process in textile production. However, before the yarn/fabric finishing, such as dyeing, the paste adhering to the warp must be eliminated to ensure optimal dyeing properties and the flexibility of the fabric. Therefore, the sizing will often consume a lot of energy and produce a lot of industrial wastewater, which will cause serious harm to the environment. In this study, we have developed an energy saving and environmentally friendly starch-based slurry by modifying natural starch with acrylamide. The paste has excellent viscosity stability and fiber adhesion, and exhibits excellent performance during warp sizing. In addition, the slurry has good water solubility at 60-70 °C, so it is easy to desize at low temperatures. Because of this, the sizing of the warp can be deslimed directly from the yarn during subsequent washing processes. This work can not only reduce some costs for the textile industry, but also achieve the purpose of energy conservation and emission reduction.
Related Concept Videos
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the...
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...