The Application of Box-Behnken Design for Investigating the Supercritical CO2 Foaming Process: A Case Study of
Salal Hasan Khudaida1, Shih-Kuo Yen1, Chie-Shaan Su1
1Department of Chemical Engineering and Biotechnology, National Taipei University of Technology, Taipei 10608, Taiwan.
Abstract:
Thermoplastic polyurethane (TPU) is a versatile polymer with unique characteristics such as flexibility, rigidity, elasticity, and adjustable properties by controlling its soft and hard segments. To properly design and understand the TPU foaming process through supercritical CO2, a design of experiments approach, the Box-Behnken design (BBD) was adopted using commercial TPU 85A as the model compound. The effect of saturation pressure, saturation temperature, and immersion time on the mean pore size and expansion ratio were investigated. The design space for the production of TPU foam was shown, and the significance of process parameters was confirmed using the analysis of variance (ANOVA). In addition, extrapolation foaming experiments were designed and validated the feasibility of the response surface model developed via BBD. It was found that the pore size of TPU 85A foam could be controlled within 13 to 60 μm, and a stable expansion ratio could be designed up to six.
More Related Videos
09:16Author Spotlight: Optimization of Processing Technology for Tiebangchui with Zanba Based on CRITIC Combined with Box-Behnken Response Surface Method
Published on: May 12, 2023
09:12Optimization of Processing of Tiebangchui with Highland Barley Wine Based on the Box-Behnken Design Combined with the Entropy Method
Published on: May 19, 2023
Related Concept Videos
Molecular Weight of Step-Growth Polymers
As the step-growth polymerization involves step-wise condensation of monomers, the molecular weight also builds up eventually. Consequently, high molecular weight polymers are obtained at the late stages of the polymerization, where 99% of monomers have been consumed.
The extent of the...
Turbulent Flow: Problem Solving
Temperature is a key factor in CO2 solubility. In this case, the CO2 gas and the liquid are cooled to 20°C. Lower temperatures...