Abstract:
Two-dimensional (2D) materials are attracting attention because of their outstanding physical, chemical, and electrical properties for applications of various future devices such as back-end-of-line field effect transistor (BEOL FET). Among many 2D materials, tin disulfide (SnS2) material is advantageous for low temperature process due to low melting point that can be used for flexible devices and back-end-of-line (BEOL) devices that require low processing temperature. However, low temperature synthesis method has a poor crystallinity for applying to various semiconductor industries. Hence, many studies of improving crystallinity of tin disulfide film are studied for enhancing the quality of film. In this work, we propose a precursor multi-dosing method before deposition of SnS2. This precursor pre-treatment was conducted by atomic layer deposition cycles for more adsorption of precursors to the substrate before deposition. The film quality was analyzed by x-ray diffraction, Raman, transmission electron microscopy, atomic force microscopy and x-ray photoelectron spectroscopy. As a result, more adsorbates by precursor pre-treatment induce higher growth rate and better crystallinity of film.
More Related Videos
14:01Making Record-efficiency SnS Solar Cells by Thermal Evaporation and Atomic Layer Deposition
Published on: May 22, 2015
08:50Preparation of Large-area Vertical 2D Crystal Hetero-structures Through the Sulfurization of Transition Metal Films for Device Fabrication
Published on: November 28, 2017
Related Concept Videos
Preparation and Reactions of Sulfides
Preparation of Samples for Electron Microscopy