Atomic layer deposition of SnS2film on a precursor pre-treated substrate

Jungtae Kim1, Dowwook Lee2, Jangho Bae2

  • 1Department of Nanoscale Semiconductor Engineering, Hanyang University, Seoul, 04673, Republic of Korea.

Nanotechnology
|February 2, 2024
PubMed