Mechanical behavior and waterproof performance of longitudinal section of tunnel segment joint gasket

Qian Zhang1, Li Xie2, Zhirong Zhao3

  • 1Shijiazhuang Tiedao University, Shijiazhuang, 050043, China.

Scientific Reports
|May 8, 2024
PubMed

Related Concept Videos

Waterproofing and Anti-Bacterial Admixtures in Concrete01:22

Waterproofing and Anti-Bacterial Admixtures in Concrete

Concrete's susceptibility to water absorption is due to the capillary action within the pores of its hydrated cement paste. This action draws water in, creating the need for waterproofing admixtures to prevent such penetration. The efficacy of these admixtures is contingent upon the water pressure, with variations arising from different conditions such as rain, capillary rise, or hydrostatic pressure in structures intended to hold water.
Waterproofing admixtures render concrete hydrophobic,...
77
Types of Building Separation Joints01:23

Types of Building Separation Joints

Building separation joints divide large or complex building structures into smaller, discrete units that can move independently. These joints are categorized into three types: volume-change joints, settlement joints, and seismic separation joints.
Volume-change joints address the effects of expansion and contraction due to temperature and moisture variations. They are strategically placed at discontinuities in a building's mass where cracking is most likely and are spaced about 150 to 200...
211
Design Example: Joints in Concrete Pavements01:28

Design Example: Joints in Concrete Pavements

Concrete pavement joints are essential for maintaining the structural integrity and longevity of pavement by controlling where and how the pavement cracks. These joints can be categorized based on their functions, such as contraction or control joints, construction joints, isolation joints, and expansion joints.
Contraction joints are typically formed by sawing a groove into the concrete shortly after it has hardened. This creates a weakened vertical plane, deliberately encouraging cracking at...
181
Masonry in Cold and Hot Weather Conditions01:21

Masonry in Cold and Hot Weather Conditions

In cold weather, masonry construction requires specific precautions to ensure mortar does not freeze before curing, as this can significantly weaken its strength and watertightness. Mortar temperature should be maintained between 60°F and 80°F to support proper hydration and curing. Below 40°F, mortar water must be heated, but should not exceed 120°F as high temperatures can reduce mortar's compressive and bond strength.
Other key practices include keeping masonry units...
83
Mortar Joint Deterioration in Masonry01:13

Mortar Joint Deterioration in Masonry

Mortar joint deterioration is a significant concern in masonry structures, with water accumulation in the joints leading to damage from freeze-thaw cycles. The repeated expansion of water during freezing and its melting during thawing develop and propagate cracks in the masonry joints. Eventually, this leads to the spalling of mortar from the joints, loosening masonry units and weakening the structure. The deteriorated mortar joints are also vulnerable to moisture intrusion into the walls.
The...
114
Permeability of Concrete01:25

Permeability of Concrete

Permeability in the context of concrete refers to how easily liquids or gases can pass through the material. This quality is crucial for assessing the water-tightness and durability of concrete structures and their resistance to chemical attacks. Concrete permeability can be determined through comparative laboratory tests. These tests typically involve sealing a concrete specimen from the sides, applying water pressure to the top surface with pressure, and measuring the amount of water passing...