Assessment of modified chitosan composite in acidic reservoirs through pilot and field-scale simulation studies

Hamid Khattab1, Ahmed A Gawish1, Sayed Gomaa2,3

  • 1Petroleum Engineering Department, Faculty of Petroleum & Mining Engineering, Suez University, Cairo, Egypt.

Scientific Reports
|May 9, 2024
PubMed

Related Concept Videos

Quality of Water01:19

Quality of Water

In concrete preparation, the quality of water is paramount as it affects the strength and durability of the concrete. Potable water is usually preferred; however, it must not have excessive sodium or potassium to prevent compromising the concrete's integrity. Water quality is typically evaluated based on impurities such as dissolved solids, chlorides, and sulfates, and its pH value is ideally between 6 and 8. Even slightly acidic natural water may be acceptable unless it contains harmful...
Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
Waterproofing and Anti-Bacterial Admixtures in Concrete01:22

Waterproofing and Anti-Bacterial Admixtures in Concrete

Concrete's susceptibility to water absorption is due to the capillary action within the pores of its hydrated cement paste. This action draws water in, creating the need for waterproofing admixtures to prevent such penetration. The efficacy of these admixtures is contingent upon the water pressure, with variations arising from different conditions such as rain, capillary rise, or hydrostatic pressure in structures intended to hold water.
Waterproofing admixtures render concrete hydrophobic,...
Carbonation Shrinkage01:24

Carbonation Shrinkage

Atmospheric CO2 penetrates the concrete's pores and, in the presence of moisture, forms carbonic acid, which then reacts with calcium hydroxide in the hydrated cement, forming calcium carbonate. This process reduces the concrete's volume and is termed carbonation shrinkage.
The concrete's permeability is slightly reduced as calcium carbonate produced during the reaction fills its pores. Furthermore, its strength is slightly enhanced as the water released during the reaction facilitates the...
Acid Attack on Concrete01:21

Acid Attack on Concrete

When acids come into contact with concrete, they initiate a chemical reaction that dissolves the hydrated cement paste. This process leads to softening and structural weakening of the concrete. This issue is commonly observed in environments such as chimneys, sewers, and industrial settings. The severity of the damage increases as the pH of the water interacting with the concrete drops below 6.5. In particular, a pH under 4.5 can cause significant concrete damage.
The rate at which hydrogen...
Alkali Aggregate Reaction in Concrete01:26

Alkali Aggregate Reaction in Concrete

The alkali-aggregate reaction in concrete involves natural siliceous minerals in aggregates reacting with alkaline hydroxides derived from cement alkalis. This reaction forms an alkali-silica gel that absorbs water, swells, and increases in volume, which is confined by the surrounding cement paste, creating internal pressures that crack and disrupt the concrete. The extent of expansion and damage can be partly attributed to the alkali-silica reaction's osmotic hydraulic pressure and the...