Related Experiment Video
Updated: Jun 25, 2025

Production and Analysis of Sporosarcina pasteurii Biocement Bricks Using Custom 3D-Printed Molds for Unconfined Compression Tests
Published on: March 7, 2025
Enhancing geomechanical characteristics of calcium sulfoaluminate (CSA) cement-treated soil under low confining
James Innocent Ocheme1, Jong Kim1, Sung-Woo Moon2
1Department of Civil and Environmental Engineering, Nazarbayev University, 53 Kabanbay Batyr Ave, 010000, Astana, Kazakhstan.
Abstract:
This study examines the efficacy of employing calcium sulfoaluminate (CSA) cement, an environmentally friendly binder, for enhancing the geomechanical characteristics of sand, particularly under low confining pressure conditions. A series of triaxial consolidated drained tests were performed on sand samples treated with varying content (5, 7, and 10%) of CSA cement and 10% ordinary Portland cement (OPC) under various low confining pressures (50, 100, 200, and 400 kPa). The test findings demonstrated the importance of cement content and confining pressure on the mode of failure, stress-strain and volumetric behavior, failure characteristics, and shear strength parameters of the treated quartz sand. After a curing period of 14 days, samples treated with 10% CSA cement exhibited a remarkable 212% increase in peak deviator stress and an 89% reduction in axial strain at failure, indicating higher initial stiffness compared to untreated samples under a 400 kPa confining pressure. Furthermore, the samples treated with 10% CSA exhibited higher peak deviator stress, initial stiffness, and strength development compared to those treated with 10% OPC. The scanning electron microscopy analysis provides insights into particle breakage and bond degradation processes, which increase with confining pressure in CSA-treated samples. Also, the mode of failure analysis reveals a transition from ductile to slightly brittle behavior with increasing cement content. Notably, the geomechanical properties of the treated material emphasized the significant impact of CSA cement on soil improvement. Thus offering a sustainable alternative for soil improvement in construction projects.
Related Concept Videos
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Types of Cement I
Type I (Ordinary Portland Cement) is widely used for general construction where special properties are not required. It has moderate sulfate resistance and heat of hydration.
Type II (Modified Cement) offers moderate resistance to sulfate attack and a lower rate of heat development compared to Type I. It is suitable for structures in...
Water Cement Ratio
Bonding and Strength of Aggregate
Soundness of Cement
Hydration of Cement