Engineered Cementitious Composites with Super-Sulfated Cement: Mechanical, Physical, and Durability Performance
Related Experiment Video
Updated: Jun 25, 2025

Preparation of Aligned Steel Fiber Reinforced Cementitious Composite and Its Flexural Behavior
Published on: June 27, 2018
Shahin Zokaei1, Hocine Siad1, Mohamed Lachemi1
1Department of Civil Engineering, Toronto Metropolitan University, Toronto, ON M5B 2K3, Canada.
Abstract:
This study aimed to bridge a research gap by exploring the utilization of super-sulphated cement (SSC) in engineered cementitious composites (ECCs) as a sustainable alternative to ordinary Portland cement (OPC)-based mixtures. The SSC was designed with slag, gypsum, and a small amount of OPC. The primary objective was to investigate the effects of incorporating SSC, both with and without fly ash (FA), at various FA/SSC ratios between 0 and 1.5. A comprehensive evaluation was conducted to assess the performance of the ECC-SSC mixtures, including the compressive and flexural strengths, ductility, ultrasonic pulse velocity, rapid chloride permeability, and drying shrinkage. Additionally, advanced microstructural evaluation techniques such as scanning electron microscopy (SEM) with energy dispersive X-ray (EDX) analysis as well as X-ray diffraction (XRD) analysis were employed to analyze the reaction products in selected mixtures. The results showed that the ECC mixture produced with SSC exhibited comparable strength to the ECC-OPC. In general, all the SSC-based ECCs fulfilled the criteria for various engineering applications, especially when the fly ash to SSC ratios were 0 and 0.8. In addition, ECCs with FA/SSC ratios of 1.2 and 1.5 showed ultra-ductile performance higher than the control ECC. Interestingly, all the FA-based ECC-SSC presented lower shrinkage characteristics than the control OPC-based ECC.
More Related Videos
05:38Production and Analysis of Sporosarcina pasteurii Biocement Bricks Using Custom 3D-Printed Molds for Unconfined Compression Tests
Published on: March 7, 2025
06:27Expression of Cementitious Pore Solution and the Analysis of Its Chemical Composition and Resistivity Using X-ray Fluorescence
Published on: September 23, 2018
Related Concept Videos
Superplasticizers
Types of Cement II
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in...
Types of Cement I
Type I (Ordinary Portland Cement) is widely used for general construction where special properties are not required. It has moderate sulfate resistance and heat of hydration.
Type II (Modified Cement) offers moderate resistance to sulfate attack and a lower rate of heat development compared to Type I. It is suitable for structures in...
Fiber Reinforced Concrete
Sulfate Attack on Concrete
Sulfates from sources like soil, groundwater, or industrial effluents...