Corrosion of Reinforcement01:27

Corrosion of Reinforcement

The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
174
Prestressed Concrete01:20

Prestressed Concrete

Prestressed concrete is a construction technique designed to enhance the strength and durability of concrete structures. This method involves the application of a pre-set tension to high-strength steel strands used as reinforcement before the concrete is subjected to its working loads. The primary aim of prestressing is to place the concrete in a state of compression, in order to counteract the tensile forces it will experience in service. This pre-compression helps prevent crack formation in...
127
Effect of Sea Water on Concrete01:22

Effect of Sea Water on Concrete

Concrete exposed to seawater can undergo degradation like the dissolution of ettringite and gypsum, increasing the material's porosity and decreasing its strength. In contrast, the crystallization of salts within the concrete's pores can cause expansion, particularly above the waterline where evaporation occurs. Nonetheless, this expansion only happens when seawater, enabled by the concrete's permeability, manages to infiltrate the structure.
Concrete in areas between tide marks,...
214
Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
105
Sulfate Attack on Concrete01:29

Sulfate Attack on Concrete

Sulfate attack on concrete is a deterioration process characterized by a whitish discoloration beginning at the edges and corners, accompanied by cracking and spalling. This phenomenon occurs when sulfates react with the components of hardened concrete, forming compounds like calcium sulfate and calcium sulfoaluminate which occupy more space than the substances they replace, causing the concrete to expand and disrupt.
Sulfates from sources like soil, groundwater, or industrial effluents...
130
Posttensioned Masonry Walls01:15

Posttensioned Masonry Walls


Post-tensioned masonry walls use high-strength steel rods or flexible tendons to enhance the strength and efficiency of masonry structures. These elements are securely anchored to the foundation and extend vertically either within the cores of the masonry units or between the masonry wythes. The construction process involves building the wall with these tensioning elements in place and allowing the mortar to fully cure.
Following the curing process, the tensioning begins. Steel rods are...