Related Experiment Video
Updated: Jun 21, 2025

Non-aqueous Electrode Processing and Construction of Lithium-ion Coin Cells
Published on: February 1, 2016
Materials recovery from NMC batteries with water as the sole solvent
Anirudha Karati1, Prashant P Gargh2, Sabyasachi Paul2
1Ames National Laboratory of US DOE, Ames, IA, 50011, USA.
Abstract:
We report an environmentally benign recycling approach for large-capacity nickel manganese cobalt (NMC) batteries through the electrochemical concentration of lithium on the anode and subsequent recovery with only water. Cycling of the NMC pouch cells indicated the potential for maximum lithium recovery at a 5C charging rate. The anodes extracted from discharged and disassembled cells were submerged in deionized water, resulting in lithium dissolution and graphite recovery from the copper foils. A maximum of 13 mg of lithium salts per 100 mg of the anode, copper current collector, and separator was obtained from NMC pouch cell cycled at a 4C charging rate. The lithium salts extracted from batteries cycled at low C-rates were richer in lithium carbonate, while the salts from batteries cycled at high C-rates were richer in lithium oxides and peroxides, as determined by X-Ray photoelectron spectroscopy. The present method can be successfully used to recover all the pouch cell components: lithium, graphite, copper, and aluminum current collectors, separator, and the cathode active material.
More Related Videos
09:50Electrochemically and Bioelectrochemically Induced Ammonium Recovery
Published on: January 22, 2015
10:31Detection and Recovery of Palladium, Gold and Cobalt Metals from the Urban Mine Using Novel Sensors/Adsorbents Designated with Nanoscale Wagon-wheel-shaped Pores
Published on: December 6, 2015