A Water Environment-Based Simulated Method for Ultrasonic Testing of Slag Inclusion Weld Defects Based on Improved

Jing Zhang1,2, Guocai Zhang3, Zijie Chen1

  • 1School of Computer Science and Engineering, Faculty of Innovation Engineering, Macau University of Science and Technology, Macau 999078, China.

PubMed