Thermo-Mechanical Properties and Phase-Separated Morphology of Warm-Mix Epoxy Asphalt Binders with Different Epoxy
Chengwei Wu1, Haocheng Yang1, Xinpeng Cui1
1MOE Key Laboratory of High Performance Polymer Materials and Technology, School of Chemistry and Chemical Engineering, Nanjing University, Nanjing 210093, China.
Abstract:
The performance and phase-separated microstructures of epoxy asphalt binders greatly depend on the concentration of epoxy resin or bitumen. In this paper, the effect of the epoxy resin (ER) concentration (10-90%) on the viscosity, thermo-mechanical properties, and phase-separated morphology of warm-mix epoxy asphalt binders (WEABs) was investigated using the Brookfield rotational viscometer, differential scanning calorimetry (DSC), dynamic mechanical analysis (DMA) and laser scanning confocal microscopy (LSCM). Due to the high reactivity of epoxy resin, the viscosity of WEABs increases with time. Furthermore, the initial viscosity of WEABs decreases with the ER concentration. Depending on the ER concentration, the viscosity-time behavior of WEABs is divided into three stages: slow (10-40%), fast (50-80%), and extremely slow (90%). In the slow stage, the viscosity slightly increases with the ER concentration, while the fast stage shows an opposite trend. DSC and DMA results reveal that WEABs with 10-80% ER exhibit two glass transition temperatures (Tgs) for cured epoxy resin and bitumen. Moreover, the Tgs of epoxy resin and bitumen increase with the ER concentration. However, WEAB with 90 % ER has only one Tg. LSCM observation shows that phase separation occurs in all WEABs. For WEABs containing 10-40% ER, spherical epoxy particles act as the discontinuous phase and disperse in the continuous bitumen phase. However, in WEABs with 50-90% ER, phase inversion takes place. Contrarily, bitumen particles disperse in the continuous epoxy phase. The damping properties of WEABs with the continuous epoxy phases increase with the ER concentration, while the crosslinking density shows an opposite trend. The occurrence of phase inversion results in a sharp increase in the tensile strength of WEABs. For WEABs with the continuous epoxy phases, the elongation at break increases with the ER concentration. The toughness first increases and then decreases with the ER concentration. A maximum toughness value shows at 70% ER.
Related Concept Videos
Design Example: Managing Concrete Workability
Polymer Classification: Crystallinity
Crystalline domains are the regions where polymer chains are aligned in an orderly manner and held together in proximity by intermolecular forces. For example, chains in the crystalline domains of polyethylene and nylon are bound together by van der Waals...
Hot Weather Concreting
Mitigating the heat increase in concrete can be economically achieved by shading aggregate stockpiles to prevent heating from solar radiation,...
Cold Weather Concreting
To counteract the negative impacts of cold weather, ensuring...
Mortar Properties
Accelerators
The effectiveness of calcium chloride can...