A Study on the Pre-Hardened Shrinkage Reduction of Grout Using Carbon Materials

Jeong-Bae Lee1, Seong-Soo Kim1, Young-Jun Lee2

  • 1Department of Smart Construction and Environmental Engineering, Daejin University, Pocheon 11159, Republic of Korea.

PubMed

Related Concept Videos

Shrinkage in Concrete01:27

Shrinkage in Concrete

Shrinkage in concrete is primarily due to water loss from evaporation, hydration of cement, or carbonation, leading to a reduction in volume. The volumetric contraction results in volumetric strain in concrete. However, in practice, shrinkage is measured as linear strain, which is one-third of the volumetric strain.
When concrete is still in its plastic state, it can undergo a decrease in volume by about 1% of its absolute volume. This decrease is known as plastic shrinkage. It arises either...
89
Drying Shrinkage01:21

Drying Shrinkage

When hardened concrete is exposed to air with a relative humidity of less than 100 percent, it begins to lose the free water within its capillaries. As this water evaporates, the water initially adsorbed onto the calcium silicate hydrates migrates towards these now empty spaces and eventually evaporates as well. Over time, as more water leaves, the volume of the concrete decreases, a phenomenon known as drying shrinkage.
A portion of this drying shrinkage can be reversed; if the concrete is...
74
Carbonation Shrinkage01:24

Carbonation Shrinkage

Atmospheric CO2 penetrates the concrete's pores and, in the presence of moisture, forms carbonic acid, which then reacts with calcium hydroxide in the hydrated cement, forming calcium carbonate. This process reduces the concrete's volume and is termed carbonation shrinkage.
The concrete's permeability is slightly reduced as calcium carbonate produced during the reaction fills its pores. Furthermore, its strength is slightly enhanced as the water released during the reaction...
122
Preplaced Aggregate Concrete01:29

Preplaced Aggregate Concrete

Preplaced aggregate concrete is ideal for construction environments that are not easily accessible. The process begins by properly wetting the gap-graded coarse aggregates to remove the dirt, then placing it in the form and compacting it. Voids are filled with a mortar mix pumped under pressure through slotted pipes. This mortar typically consists of Portland cement, pozzolan, fine aggregates, water, and a fluidizing aid. The pozzolan helps reduce bleeding and segregation while improving the...
95
Waterproofing and Anti-Bacterial Admixtures in Concrete01:22

Waterproofing and Anti-Bacterial Admixtures in Concrete

Concrete's susceptibility to water absorption is due to the capillary action within the pores of its hydrated cement paste. This action draws water in, creating the need for waterproofing admixtures to prevent such penetration. The efficacy of these admixtures is contingent upon the water pressure, with variations arising from different conditions such as rain, capillary rise, or hydrostatic pressure in structures intended to hold water.
Waterproofing admixtures render concrete hydrophobic,...
75
Accelerators01:17

Accelerators

Accelerators in concrete serve as admixtures to speed up the hardening process, enabling the concrete to achieve early strength faster. Although accelerators do not necessarily impact the time it takes concrete to set, they reduce this time in practice. A common accelerator is calcium chloride, which is particularly useful for hastening early strength development in cold weather or for rapid repair jobs that require quick heat generation after mixing.
The effectiveness of calcium chloride can...
71