Multidepth quantitative analysis of liver cell viscoelastic properties: Fusion of nanoindentation and finite element

Yi Zeng1,2,3, Xianping Liu4, Zuobin Wang1,2,5

  • 1International Research Centre for Nano Handling and Manufacturing of China, Changchun University of Science and Technology, Changchun, China.